TANTALUM RODS
Are supplied according to the parties agree in soft (heat-treated) or solid (not heat-treated) condition. The chemical content of rods is similar to chemical content of ingots.
Parameters
|
Item
|
Diameter, mm
|
Length, mm
|
|
Rods, made by wire-drawing, without surface turning
|
3.0 - 6.0
|
500-4000
|
|
6.0 - 8.0
|
100-2000
|
|
Rods with surface turning
|
3.0 - 15.0
|
from 300 to 2000
|
|
16 - 29
|
from 300 to 1500
|
|
30 - 50
|
from 300 to 1200
|
|
51 - 90
|
from 300 to 1000
|
The roughness of turning rods < RZ 40. According to the agreement with the customer the supply of other type and size of building elements is possible.
|
Controlled dashs, %
|
Dashs mass concentration, % not more then
|
Controlled dashs, %
|
Dashs mass concentration, % not more then
|
|
Ta, not more then
|
99,92
|
Mg
|
0,0002
|
|
Si
|
0,0012
|
Ni
|
0,0002
|
|
Fe
|
0,0012
|
Cr
|
0,00025
|
|
Mn
|
0,00015
|
Ti
|
0,0003
|
|
Sn
|
0,0001
|
Co
|
0,0001
|
|
Cu
|
0,0005
|
Na
|
0,00015
|
|
Nb
|
0,014
|
C
|
0,0050
|
|
Zr
|
0,0007
|
N
|
0,0050
|
|
Al
|
0,0005
|
O
|
0,0050
|
|
Ca
|
0,0010
|
H
|
0,0004
|
|
W
|
0,005
|
Mo
|
0,0005
|
The rod shouldn't have curves, cracks, wire-edges, exfoliations and other defects that can influence further utilization.
|
|